At Nova, we run a Just-In-Time manufacturing process which basically means that we produce material often and have tight control over the process.

Every month there are several sheets that have imperfect edges where the photopolymer layer is not adhered to the base PETG all the way to the edge of the sheet. These sheets will work fine as long as there is no raised image on this area.

The problems areas are clearly marked and represent no more than 5% of the sheet. Typically, one of the four edges has an area of approx. 1/2' where there is no photopolymer as seen below.


NovAcryl Pro Rated 236 leading edge missing 1/2" of polymer


How To Purchase Pro Rated Sheets
  • Log into the Online Ordering section on our website
  • If you do not now your log in information contact Pat Avallone
  • The Pro Rated material will be listed on the Home screen
  • Material selection will change monthly based availability
  • Material will be sold on a first come, first serve basis
Please contact us today if you have any question about the NovAcryl Pro Rated material or if you would like to set up your online account.  --MS